Add to Cart
Electrical Resistance Wire Nickel Chromium 80/20 Flat Wire Ni80 Cr20 Ribbon Wire for Electronics industy
Product Introduction
Cr20Ni80 Wire has a wide range of applications in the electronics field, mainly due to its excellent resistance properties and high temperature stability. The main components of this alloy include 20% chromium (Cr) and 80% nickel (Ni), and the combination of these components makes it perform well in high temperature and corrosive environments. The physical properties of Cr20Ni80 Wire include density 8.4 g/cm³, melting point 1400°C, resistivity at 20°C is about 1.09 Ω·mm²/m, thermal expansion coefficient (20°C-1000°C) is 17×10⁻⁶/°C, and thermal conductivity (20°C) is 15 W/m·K.
In the electronics field, Cr20Ni80 Wire is widely used to manufacture various resistance components, such as resistors, potentiometers, thermistors, etc. Its high resistivity and stable resistance characteristics enable it to generate stable heat when current passes through it, while maintaining good corrosion resistance and oxidation resistance, ensuring the reliability and safety of the equipment in long-term use. In addition, the resistance temperature coefficient of Cr20Ni80 Wire is small (<200 ppm/°C, 20°C-1000°C), which means that the change of resistance value is very small in a wide temperature range, so its resistance value has high stability, which is particularly suitable for precision instruments and constant temperature electric heating elements.
Size dimension range:
Wire: 0.01-10mm
Ribbons: 0.05*0.2-2.0*6.0mm
Strip: 0.05*5.0-5.0*250mm
NiCr series: Cr10Ni90,Cr20Ni80, Cr30Ni70, Cr15Ni60, Cr20Ni35, Cr20Ni30
Parameter
Resistivity: At 20°C, the resistivity is usually 1.09-1.20 μΩ·m.
Density: 8.4 g/cm³.
Melting point: about 1400°C.
Thermal conductivity: about 15 W/m·K (at 20°C).
Linear expansion coefficient: 14-18×10^-6/K in the range of 20°C to 1000°C.
Tensile strength: not less than 650 MPa.
Elongation: ≥20%.
Performance material | Cr20Ni80 | |
Composición | Ni | Rest |
Cr | 20.0~23.0 | |
Fe | ≤1.0 | |
Temperatura máxima℃ | 1200 | |
Punto de fusion ℃ | 1400 | |
Densidad g/cm3 | 8.4 | |
Resistividad μΩ·m,20℃ | 1.09±0.05 | |
Alargamiento a la ruptura | ≥20 | |
Calor especifico J/g.℃ | 0.44 | |
Conductividad térmica KJ/m.h℃ | 60.3 | |
Coeficiente de expansión de líneas a×10-6/(20~1000℃) | 18 | |
Estructura micrográfica | Austenite | |
Propiedades magnéticas | Nonmagnetic |
Form | Specification | |
Wire | Diameter=0.025mm~8mm | |
Flat wire | Width=0.40~6.0mm | Thick=0.03~0.50mm |
Strip | width=8~250mm | Thick=0.05~3.0mm |
Bar | Diameter=8~100mm | Long=50~1000 |
Specific Applications
Advantages and Characteristics
Contact Us
Email:fbwlau@cnrunlai.com
Oem service:
Welcome customized size
We are experience factory for OEM&ODM service
Our Nichrome Alloy product comes with technical support and services to ensure optimal performance and customer satisfaction:
We are committed to providing our customers with the highest level of support and service for our Nichrome Alloy product.
Product Packaging:
Shipping:
Related Questions and Answers
Q: What is the heat treatment process of Cr20Ni80 wire?
Answer: The heat treatment process of Cr20Ni80 wire includes annealing, solution treatment and aging treatment. Annealing temperatures are typically 800°C to 1000°C, solution treatment temperatures are 1000°C to 1150°C, followed by rapid water cooling, and aging temperatures are 450°C to 600°C. Reasonable heat treatment process can significantly improve the comprehensive properties of the alloy.
Q: What is the fatigue performance of Cr20Ni80 wire?
Answer: Cr20Ni80 wire is prone to fatigue cracks during repeated heating and cooling at high temperatures. In the rapid thermal cycle test at 1000°C and 20°C, significant micro cracks appeared on the surface of the material after 1000 cycles, accompanied by tiny peeling. As the number of cycles increases, the cracks further expand, resulting in a degradation of material properties.
Q: What is the oxidation resistance of Cr20Ni80 wire?
Answer: Cr20Ni80 wire has excellent anti-oxidation properties. Its surface can form a dense chromium oxide film at high temperature, which effectively prevents further oxidation. When heated in air, the oxide film is able to self-repair, which gives it better long-term stability at high temperatures. The anti-oxidation temperature can reach over 1100°C, especially showing good corrosion resistance in oxygen atmosphere.